Insights
POM for injection molding: homopolymer vs copolymer
Published · TECH & MORE
Injection-molding POM (acetal) is stiff, low-friction and stable. Compare POM-H vs POM-C, common brands, molding parameters and how to choose a grade.
Injection-molding POM (polyoxymethylene, also called acetal or polyacetal) is one of the most widely used engineering plastics for gears, sliding parts and precision mechanical components. It is stiff, low-friction, fatigue resistant and dimensionally stable.
Key properties of POM
- High stiffness and strength with good fatigue resistance – suited to repeated loading.
- Low friction and good wear resistance.
- Dimensional stability, with much lower moisture uptake than PA.
- Good resistance to solvents, fuels, oils and grease.
- Easy to process by both injection molding and machining.
- Food-contact grades available.
Limitations: POM does not resist strong acids, is hard to bond and print, and standard grades are only UL94 HB.
POM homopolymer (POM-H) vs copolymer (POM-C)
POM comes in two types made by different processes:
| POM-H (homopolymer) | POM-C (copolymer) | |
|---|---|---|
| Strength, stiffness | About 10–15% higher | Slightly lower |
| Thermal stability in processing | Narrower | Wider processing window |
| Chemical / hot-water resistance | Lower | Better |
| Price | Usually higher | Usually lower |
Both types work in most applications. POM-H suits thin-walled parts that need maximum stiffness; POM-C suits hot water, chemical exposure or a wider molding window.
Common POM brands
- Homopolymer: Delrin®, Tenac™ (Asahi Kasei).
- Copolymer: DURACON® (Polyplastics), Hostaform® / Celcon® (Celanese), KEPITAL® (KEP), Ultraform® (BASF), Tenac™-C (Asahi Kasei), Iupital® (Mitsubishi Engineering-Plastics), Formocon (Formosa).
Each brand offers many grades: standard, high-flow, impact-modified, glass-filled, low-friction, antistatic and low-emission (low VOC) for vehicle interiors.
For advice and help choosing the right grade, please contact TECH & MORE – Hotline/Zalo: +84 375 181318 · Email: mark@technmore.com.vn
Typical applications
- Gears, worm gears and cams in machinery and appliances.
- Bearings, bushings and rollers.
- Clips, latches, plastic springs and fasteners.
- Automotive fuel-system parts, door mechanisms, seat-belt components.
- Faucets, valves and water-contact parts.
Typical injection molding parameters
| Parameter | Typical value |
|---|---|
| Drying | 80–100 °C, 2–4 hours (if pellets are damp) |
| Melt temperature | 190–210 °C (POM-H slightly higher than POM-C) |
| Mold temperature | 60–90 °C |
Do not exceed 230 °C or leave POM in the barrel for long – it degrades and releases formaldehyde. Exact values follow each grade’s TDS – TECH & MORE provides it with trial samples.
Tips for choosing and molding POM
- Check the operating temperature and chemical environment (especially acids and chlorinated hot water).
- High-wear gears can use low-friction POM or be combined with injection-moldable UHMWPE.
- Avoid long residence time of molten resin in the barrel to prevent degradation.
- Design uniform wall thickness to limit shrinkage and voids.
See typical data on our POM resin page, or send a request and TECH & MORE will recommend a grade and send samples.
For advice and help choosing the right grade, please contact TECH & MORE.
Hotline/Zalo: +84 375 181318 · mark@technmore.com.vn